MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Superwool®Plus Expanding Paper Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool ® Plus Expanding Paper is a thin, flexible material that expands on heat exposure to provide thermal insulation and fire protection when exposed to fire or heat. The expansion ratio can be engineered within the range of: 3:1 to 12:1 to suit application requirements. The expansion property results from the use of stabilized graphite within the paper manufactured using Thermal Ceramics low biopersistence Superwool ® fibres to provide a range of refractory and thermal insulation performance. The product is normally incorporated into engineered fire-rated components to provide a sealing function during fire exposure. Typical end-use applications are: Glazing screens, Pipe wraps, Fire doors industrial, Fire rated services, Fire rated grills, Fire rated electrical boxes / down lights, Fire rated air conditioning units.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.240 - 0.320 g/cc+/- 10%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF7067 / 203366

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.