MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kinlead HSD13 Normal Grade Heat Sealable Film (thickness: 25 µm)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: HSD13 is a metalizing, normal grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side has corona treatment with a normal sealing temperature. It is widely used in food packaging for metallization.

Information provided by Kinlead.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.0 microns0.984 mil± 2.5%; ASTM-252-78
Linear Mold Shrinkage 0.030 cm/cm0.030 in/inASTM-D1204
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inASTM-D1204
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 185 %185 %ASTM-D882
Film Elongation at Break, TD 65 %65 %ASTM-D882
Coefficient of Friction 0.400.40T/T-US; ASTM-D1894
 0.400.40T/O-US; ASTM-D1894
Film Tensile Strength at Break, MD 140 MPa20300 psiASTM-D882
Film Tensile Strength at Break, TD 280 MPa40600 psiASTM-D882
Heat Seal Strength 517.9 g/25 mm1.142 lb/inKinlead
Heat Seal Strength Initiation Temperature 115 - 120 °C239 - 248 °FKinlead
 
Optical PropertiesMetricEnglishComments
Haze 1.7 %1.7 %ASTM-D1003
Gloss 92 %92 %ASTM-D1003
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
Wetting Tension (Dyne)38ASTM-D2578
Yield (m²/kg)44Kinlead

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKINL076 / 107426

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.