System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced
Material Notes:
PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.143
g/cc
ISO 1183
Linear Mold Shrinkage, Flow
0.0114
cm/cm
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0122
cm/cm
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Mechanical Properties
Original Value
Comments
Puncture Resistance
3730
N
@Temperature 23.0 °C
ISO 6603-2
4630
N
@Temperature -30.0 °C
ISO 6603-2
Ball Indentation Hardness
151
MPa
ISO 2093-1
Tensile Strength at Break
80.0
MPa
5 mm/min; ISO 527-1,-2
Tensile Strength, Yield
94.0
MPa
50 mm/min; ISO 527-1,-2
Elongation at Break
10 %
Nominal, 50 mm/min; ISO 527-1,-2
11 %
5 mm/min; ISO 527-1,-2
Elongation at Yield
4.2 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
3500
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
127
MPa
2 mm/min; ISO 178-A
Flexural Yield Strength
105
MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
3200
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
6.2 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
80.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
110
kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched
110
kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
120
kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
<=
10.0
kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
Puncture Energy
5.10
J
@Temperature -30.0 °C
ISO 6603-2
13.1
J
@Temperature 23.0 °C
ISO 6603-2
Electrical Properties
Original Value
Comments
Comparative Tracking Index
400
V
Solution B; IEC 60112
600
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
70.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point
265
°C
10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air
249
°C
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
210
°C
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
75.0
°C
ISO 75-1,-2
Deflection Temperature at 8.0 MPa
60.0
°C
ISO 75-1,-2
Vicat Softening Point
>=
230
°C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94
V-2
@Thickness 0.750 mm
Oxygen Index
30 %
Method A; ISO 4589-2
Glow Wire Ignition Temperature
775
°C
@Thickness 0.750 mm
IEC 60695-2-13
775
°C
@Thickness 1.50 mm
IEC 60695-2-13
775
°C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Thickness 1.00 mm
IEC 60695-2-12
Shrinkage, MD
0.42 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD
0.11 %
@Treatment Temp. 120 °C,
Time 14400 sec
60x60x2; ISO 294-4
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
injection molding
260
-
270
°C
Mold Temperature
80.0
°C
injection molding
80.0
-
100
°C
Drying Temperature
80.0
°C
Dry Time
2.00
-
6.00
hour
Moisture Content
0.030 - 0.070 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
Asahi Kasei Thermylon® N3-25FG-2726 PA66-GF25
EMS-Grivory Grilon® AG-25 HM PA66-GF25
PLANW9480 / 208335
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.