MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Kennametal Stellite Tribaloy® 745
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Age-hardened, highly alloyed, nickel base alloy in the casting form. Hardened by the presence of intermetallic compounds in the highly alloyed matrix. Unique combination of corrosion and wear resistant.

Applications: Used in high temperature, highly corrosive environments where good wear resistance in needed.

Data provided by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 383383Converted from Rockwell C hardness.
Hardness, Knoop 460460Converted from Rockwell C hardness.
Hardness, Rockwell A 7171Converted from Rockwell C hardness.
Hardness, Rockwell C 37 - 4637 - 46
Hardness, Vickers 405405Converted from Rockwell C hardness.
Tensile Strength, Ultimate 600 MPa87000 psi
Elongation at Break <= 1.0 %<= 1.0 %
Compressive Yield Strength 1500 MPa218000 psi
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 26 %26 %
Iron, Fe <= 2.0 %<= 2.0 %
Molybdenum, Mo 26 %26 %
Nickel, Ni 44.5 %44.5 %As Remainder
Silicon, Si <= 1.5 %<= 1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Tribaloy® T-800
Kennametal Stellite Tribaloy® T-700 Nickel Alloy
Kennametal Stellite Tribaloy® T-900
Kennametal Stellite Tribaloy® T-400 Cobalt Alloy
Kennametal Stellite Stellite® 21

NS745A / 18888

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.