Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications. Availability: Latin America, North America and South America Additive: - Anitblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications:- Compounding
- Extrusion Compounds
- Injection Molding
- Molding Compounds
Information provided by ExxonMobil |