MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Synthos 500FRN/PL Flame retardant Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade; Polystyrene, Flame Retardant

Material Notes: Characteristics: InVento Optima 500FRN/PL and 800FRN/PL is expandable polystyrene (EPS) based on innovative thermal additive, with a low thermal conductivity value. The materials was produced using recycled materials. Materials have a form of grey spherical polystyrene particles that contain a new type of flame retardant pFR (without HBCD) and low level of hydrocarbon as a blowing agent. Their surface is coated to support processing and to prevent electrostatic charge. Due to the content of halogenated flame retardant the product is unsuitable for objects intended for direct contact with food.

Information provided by Synthos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0130 - 0.0400 g/cc0.000470 - 0.00145 lb/in³raw material
 <= 0.180 g/cc<= 0.00650 lb/in³
 0.595 - 0.690 g/cc0.0215 - 0.0249 lb/in³expanded beads, according to the test1)/Foamability
Particle Size 900 - 1100 µm900 - 1100 µmfraction
 800 - 1200 µm800 - 1200 µmFraction of the particle size >95 %
 
Descriptive Properties
Content<300 ppmResidual monomer content
 <5.2%Blowing agent content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSYNTHOS141 / 320422

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.