MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Melamine-Phenolic Copolymer
Categories: Polymer; Thermoset; Melamine; Melamine-Phenolic Copolymer

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 - 1.81 g/ccAverage value: 1.64 g/cc Grade Count:22
Water Absorption 0.220 - 2.50 %Average value: 1.18 % Grade Count:21
Linear Mold Shrinkage 0.00150 - 0.0130 cm/cmAverage value: 0.00744 cm/cm Grade Count:22
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 67.0 - 86.0Average value: 75.8 Grade Count:11
Tensile Strength, Ultimate 53.0 - 76.0 MPaAverage value: 61.7 MPa Grade Count:12
Tensile Strength, Yield 40.0 - 90.0 MPaAverage value: 61.0 MPa Grade Count:10
Elongation at Break 0.470 - 0.950 %Average value: 0.745 % Grade Count:11
Modulus of Elasticity 5.00 - 13.3 GPaAverage value: 8.92 GPa Grade Count:22
Flexural Yield Strength 70.0 - 140 MPaAverage value: 101 MPa Grade Count:22
Flexural Modulus 5.00 - 14.0 GPaAverage value: 9.00 GPa Grade Count:22
Compressive Yield Strength 142 - 250 MPaAverage value: 194 MPa Grade Count:22
Izod Impact, Notched 0.159 - 0.215 J/cmAverage value: 0.186 J/cm Grade Count:11
Charpy Impact Unnotched 0.450 - 1.40 J/cm²Average value: 0.814 J/cm² Grade Count:11
 0.400 - 0.700 J/cm²
@Temperature -40.0 - -40.0 °C
Average value: 0.550 J/cm² Grade Count:1
Charpy Impact, Notched 0.120 - 0.239 J/cm²Average value: 0.180 J/cm² Grade Count:21
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+11 - 1.00e+14 ohm-cmAverage value: 1.63e+13 ohm-cm Grade Count:22
Surface Resistance 1.00e+10 - 1.00e+12 ohmAverage value: 1.04e+11 ohm Grade Count:11
Dielectric Constant 6.50 - 16.0Average value: 9.35 Grade Count:22
Dielectric Strength 4.80 - 30.0 kV/mmAverage value: 12.3 kV/mm Grade Count:21
Dissipation Factor 0.0300 - 0.500Average value: 0.160 Grade Count:22
Arc Resistance 115 - 188 secAverage value: 172 sec Grade Count:14
Comparative Tracking Index 175 - 600 VAverage value: 519 V Grade Count:22
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 - 53.0 µm/m-°C
@Temperature 40.0 - 130 °C
Average value: 29.6 µm/m-°C Grade Count:12
Thermal Conductivity 0.400 - 0.600 W/m-KAverage value: 0.470 W/m-K Grade Count:10
 0.510 - 0.610 W/m-K
@Temperature 100 - 100 °C
Average value: 0.570 W/m-K Grade Count:4
Maximum Service Temperature, Air 135 - 190 °CAverage value: 150 °C Grade Count:22
Deflection Temperature at 1.8 MPa (264 psi) 155 - 202 °CAverage value: 178 °C Grade Count:21
Deflection Temperature at 8.0 MPa 110 - 140 °CAverage value: 123 °C Grade Count:11
Flammability, UL94 V-0 - 5VBGrade Count:21
Oxygen Index 33.0 - 36.0 %Average value: 34.2 % Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material
Overview of materials for Phenolic; Unreinforced; Molded
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength

O2369a / 89073

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.