MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reade Advanced Materials Bentonite Powder (BaTiSi3O9)
Categories: Ceramic; Clay

Material Notes: A rock composed essentially of a crystalline clay-like mineral formed by devitrification and the accompanying chemical alteration of a glassy igneous material, usually a tuff or volcanic ash.
Used as a foundry sand, paints, fuller's earth, drilling mud, bleaching clay, filtering agents, water impedance, inks, additive to ceramic materials, and iron ore pelletizing. Used in pharmaceuticals, beverage, food, cosmetics, and personal care products (Suspending agent, gellant and binder). Bentonite possesses thixotropic properties and deposits a thin water proofing film on the walls of the bore holes & thus renders permeable formations impermeable. Both natural & synthetic Bentonite are used in preparation of drilling muds. It is mainly used as circulation mud in rotary system of drilling for oil. The main purpose of Bentonite is to lubricate & cool the rotary cutting bits, carry away rock cutting fragments & to act as a seal against the escape of gas from the bore hole & to improve & prevent the hole from blowing out. Another function of such Bentonite based fluids is to condition the wall of the drill hole to prevent caving.

Numerous particle size options are available in the lower micron area from a mean particle size of 2.5 to 4.0 microns.

Information provided by Reade Advanced Materials.

Key Words: BaTiSi3O9, taylorite, fuller's earth, Wyoming sodium bentonite, sodium montmorillonite, saponite, hectorite, hormite clay
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Density 0.761 g/cc0.0275 lb/in³
pH 8.5 - 10.58.5 - 10.5
Specific Surface Area 100 - 360 m²/g100 - 360 m²/g
 
Descriptive Properties
Colorlight cream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hard Foundry Type Alloy (UNS L53710)
Bohler-Uddeholm UDDEHOLM Carmo Granshots Tool Steel Foundry Meltstock
BCC Products MB 4000 RED Urethane Foundry Plank
CMT Materials REN Shape® 5169 Foundry Pattern Board
Hard Foundry Type Alloy (UNS L53780)

CREADE001 / 1935

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.