MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Superior Preflux Nickel Cleaner
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Description: Superior PreFlux Nickel Cleaner was specially formulated to remove oxides from Nickel and Nickel-based alloys prior to lead tinning or soldering. The Superior PreFlux Nickel Cleaner is a waterbased acid cleaner that can be used immediately prior to any lead or lead frame tinning operation.

Application: Prior to using the Superior PreFlux Nickel Cleaner, it is recommended that any organic film such as oil, grease, or others be removed from the surface. This may be accomplished by using a solvent vapor degreaser or an aqueous cleaning system using the Superior SyberKleen 2000 in a 10% concentration. To remove the oxide, the Nickel or Nickel alloy components should be dipped in the Superior PreFlux Nickel Cleaner a period of 1-30 seconds depending on the degree of oxidation. Room temperature or heated PreFlux Cleaner (up to 60°C/140°F) is recommended. The components should then be rinsed in clean water to remove post-dipping residues prior to tinning.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 - 1.15 g/cc
Density 9.18 lb/gal
pH >= 1.0
 
Descriptive Properties
ColorClear, Green
Conductivity400-450 Mv

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlson 70 30 Cu Ni Copper-Nickel Alloy
International Mold Steel DC53 General-Purpose Cold Work Die and Mold Steel
Epoxy Technology EPO-TEK® H20-FC Electrically Conductive Epoxy
Carlson 90 10 Cu Ni Copper-Nickel Alloy
Aperam CuNi 44 Resistant Alloys Copper-Nickel Alloys

NSFLUX122 / 185806

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.