MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Firelite BM G Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Insulating Aggregate / Vermiculite. Bond type: Hydraulic.

Description: An extremely strong insulating concrete for service up to 1370°C/2500°F. Designed for use in those areas that require a combination of light weight and high strength. It can be cast or gunned. Particularly used in petrochemical stills and as heater linings and for furnace doors, covers, kiln car tops, etc. Conforms to classes Q and R; ASTM classification C-401-84.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.540 g/cc0.0195 lb/in³dried to 110°C
Grain Size <= 8000 µm<= 8000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  0.700 MPa
@Treatment Temp. 815 °C
102 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 1.00 MPa
@Treatment Temp. 110 °C
145 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.110 W/m-K
@Temperature 200 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 392 °F
ASTM C417
 0.140 W/m-K
@Temperature 400 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C417
Maximum Service Temperature, Air <= 870 °C<= 1600 °F
Shrinkage 1.0 %
@Treatment Temp. 815 °C
1.0 %
@Treatment Temp. 1500 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 24.7 %24.7 %
CaO 22.7 %22.7 %
Fe2O3 7.3 %7.3 %
K2O+Na2O 9.9 %9.9 %
SiO2 32.6 %32.6 %
TiO2 0.80 %0.80 %
 
Descriptive Properties
Net Material Required (kg/m³)490
Water Addition[110 % by weight]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6052 / 202836

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.