MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
GRECO ISOTANE® 5055D Polyether TPU Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Characteristics: ISOTHANE® 5000 SERIES products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility according to USP class VI hydrolytic resistance, fungus resistance and low temperature performance properties. ISOTHANE® 5000 series can be injection molded, blow molded and extruded.

Application: Medical Tubing and Medical Disposable Applications

Information provided by Great Eastern Resins Industrial Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57ASTM D2240
Tensile Strength 51.0 MPaASTM D412
Elongation at Break 400 %ASTM D412
50% Modulus 25.0 MPaASTM D412
100% Modulus 31.0 MPaASTM D412
300% Modulus 48.0 MPaASTM D412
Flexural Modulus 134 MPaASTM D792
Tear Strength 225 kN/mDie C; ASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGRECO5193 / 282176

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.