MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sumitomo Bakelite Durez® 33134 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez® 33134 is a water based, thermosetting phenolic resin of the one step type (resole). Durez® 33134 is developed to serve as basic bonding material in the manufacturing of phenolic foam. Addition of tension-active components, blowing agent and catalyst are required to generate the requested foam properties.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 75 %
@Load 0.00300 kg,
Temperature 135 °C
75 %
@Load 0.00661 lb,
Temperature 275 °F
1 hr; DCT 156
Water Absorption 17 %17 %DCT 74
pH 8.08.0DCT 46
Viscosity Measurement 2100
@Temperature 25.0 °C
2100
@Temperature 77.0 °F
DCT 61
 
Descriptive Properties
Free Formaldehyde Content, %0.3DCT 166
Free Phenol, %6DCT 431

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUMIT277 / 194082

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.