MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 357.0-T6, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 357.0-T6; UNS A03570; AA357.0-T6; Al357.0-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.67 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 75 - 105AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 114Estimated from Brinell Hardness.
Hardness, Rockwell A 37Estimated from Brinell Hardness.
Hardness, Rockwell B 56Estimated from Brinell Hardness.
Hardness, Vickers 101Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 45.0 ksiAA
Elongation at Break >= 3.0 %AA; in 2 in. (50 mm) or 4D
Tensile Modulus 72.4 GPa(A357.0)
Poissons Ratio 0.33Calculated Value(A357.0)
Machinability 50 %0-100 Scale (100=best)
Shear Modulus 26.8 GPa(A357.0)
Shear Strength 187 MPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000440 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 21.4 µm/m-°C
@Temperature 20.0 - 100 °C
 23.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.963 J/g-°C
Thermal Conductivity 151 W/m-K
Melting Point 557 - 613 °C
Solidus 557 °C
Liquidus 613 °C
 
Processing PropertiesOriginal ValueComments
Solution Temperature 1005 °Fhold at temperature for 8 hr; hot water quench
Aging Temperature 340 °Fhold at temperature 3 to 5 hrs
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 91.2 - 93.1 %As remainder
Copper, Cu <= 0.05 %
Iron, Fe <= 0.15 %
Magnesium, Mg 0.45 - 0.60 %
Manganese, Mn <= 0.03 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si 6.5 - 7.5 %
Titanium, Ti <= 0.20 %
Zinc, Zn <= 0.05 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 357.0-F Casting Alloy
Aluminum A357.0-T61, Permanent Mold Cast
Aluminum A357.0-T62, Cast
Aluminum 356.0-T6, Permanent Mold Cast
Aluminum A356.0-T6, Sand Cast

MAC3570T6 / 9952

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.