MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 20C Shock Absorber Strip Steel
Categories: Metal; Ferrous Metal; Special-Purpose Steel

Material Notes: The characteristics of Sandvik 20C shock absorber steel are:
  • High strength and wear resistance
  • High fatigue strength under bending and impact stress
  • Excellent surface finish
  • Low level of non-metallic inclusions
  • Good dimensional tolerances
  • Good flatness
  • Information provided by Sandvik

    ASTM 1095

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.80 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Ultimate 1750 MPa
    @Diameter 0.475 - 0.600 mm
     1800 MPa
    @Diameter 0.425 - 0.475 mm
     1850 MPa
    @Diameter 0.375 - 0.425 mm
     1900 MPa
    @Diameter 0.275 - 0.375 mm
     1950 MPa
    @Diameter 0.225 - 0.275 mm
     2000 MPa
    @Diameter 0.175 - 0.225 mm
     2050 MPa
    @Diameter 0.125 - 0.175 mm
     2100 MPa
    @Diameter <=0.125 mm
    Modulus of Elasticity 210 GPa
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 10.5 µm/m-°C
    @Temperature 30.0 - 100 °C
     11.5 µm/m-°C
    @Temperature 30.0 - 200 °C
     12.5 µm/m-°C
    @Temperature 30.0 - 300 °C
    Specific Heat Capacity 0.460 J/g-°C
    @Temperature 50.0 - 100 °C
    Thermal Conductivity 49.0 W/m-K
    @Temperature 20.0 °C
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C 1.0 %
    Chromium, Cr 0.20 %
    Iron, Fe 98.1 %As Balance
    Manganese, Mn 0.40 %
    Phosphorus, P <= 0.020 %
    Silicon, Si 0.30 %
    Sulfur, S <= 0.010 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Sandvik 20C Strip Steel
    Zinc Alloy 7; AG40B; Zn-4Al-0.015Mg; Zamak7
    Zinc AC41A Alloy (Zamak 5), As Cast
    AISI 81B45 Steel
    AISI 1005 Steel

    NSANDV284 / 19178

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.