MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio reported herein are typical of INCONEL® alloy 718SPF (not necessarily annealed samples).

Data provided by the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.296 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 24
Tensile Strength, Ultimate 162000 psi
Tensile Strength, Yield 120000 psi
@Strain 0.2 %
Elongation at Break 31 %
Modulus of Elasticity 205 GPacold-rolled, heat treated sheet
Poissons Ratio 0.284cold-rolled, heat treated sheet
Shear Modulus 80.0 GPacold-rolled, heat treated sheet
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000125 ohm-cm
Magnetic Permeability 1.0013at 200 Oersted (15.9 kA/m); Annealed
Curie Temperature <= -197 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.15 µm/m-°C
@Temperature 21.0 - 93.0 °C
Mean; Annealed and Aged
 13.77 µm/m-°C
@Temperature 21.0 - 316 °C
Mean; Annealed and Aged
 14.4 µm/m-°C
@Temperature 21.0 - 538 °C
Mean; Annealed and Aged
Specific Heat Capacity 0.435 J/g-°C
Thermal Conductivity 11.1 W/m-KAnnealed at 1800°F(982°C) for 1 h.
Melting Point 1260 - 1335 °C
Solidus 1260 °C
Liquidus 1335 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.20 - 0.80 %
Boron, B <= 0.0060 %
Carbon, C <= 0.050 %
Chromium, Cr 17 - 21 %
Cobalt, Co <= 1.0 %
Copper, Cu <= 0.30 %
Iron, Fe 19 %As remainder
Manganese, Mn <= 0.35 %
Molybdenum, Mo 2.8 - 3.3 %
Nickel, Ni 50 - 55 %Including Cobalt
Niobium, Nb (Columbium, Cb) 4.75 - 5.25 %Includes Ta
Nitrogen, N <= 0.010 %
Phosphorus, P <= 0.015 %
Silicon, Si <= 0.35 %
Sulfur, S <= 0.0020 %
Titanium, Ti 0.65 - 1.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged
Special Metals INCONEL® Alloy 718
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy
Universal Wire Works Inconel 718 (AMS 5832) Filler Metal
Special Metals INCONEL® Alloy 686 Nickel Superalloy Plate (UNS N06686)

NINCO53 / 17486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.