MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulated pattern to achieve a slip resistant surface as compared with the standard surface and other high density polyethylene marine grade products.

FEATURES AND BENEFITS

  • Stability- Grip-X is UV stabilized to endure the test of time outdoors.
  • Strength- Grip-X is made from the same strong polymer base as Seaboard, simply the toughest material available.
  • Inert- Grip-X is impervious to salt and moisture in marine environments.
  • Surface- Grip-X has a unique elastomer surface that provides additional traction in both wet and dry conditions.
  • Consistency- Grip-X is extruded for the most dimensional consistency.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D1505
Environmental Stress Crack Resistance 25 hour25 hourF50; ASTM D1693
 >= 500 hour>= 500 hourF50; ASTM D2561
Melt Index of Compound 0.70 g/10 min0.70 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050ASTM D2240
Tensile Strength, Ultimate 30.3 MPa4400 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
Flexural Modulus 1.52 GPa220 ksiASTM D790
Tensile Impact 53.4 J/cm100 ft-lb/inASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C172 °FASTM D648
Vicat Softening Point 125 °C257 °FASTM D1525
Brittleness Temperature <= -7.78 °C<= 18.0 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCPCV13 / 29085

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.