MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

RAMPF RAKU® TOOL InnoTuf® HP-2180 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Tough, abrasion resistant elastomer

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or MDI
Applications:
  • For hand-batch processing methods
Cure 1: 7 days at 77°F
Cure 2: 24 hours at 77°F + 5 hours at 150°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³Hardener; ASTM D-792
 1.07 g/cc0.0387 lb/in³Cure 1; ASTM D-792
 1.07 g/cc0.0387 lb/in³Cure 2; ASTM D-792
 1.08 g/cc0.0390 lb/in³Resin; ASTM D-792
Viscosity 340 cP340 cPHardener; ASTM D-2393
 2800 cP2800 cPMix; ASTM D-2393
 7100 cP7100 cPResin; ASTM D-2393
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inCure 1; ASTM D-2566
 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inCure 2; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75 - 8575 - 85Cure 1; ASTM D-2240
 75 - 8575 - 85Cure 2; ASTM D-2240
Tensile Strength 12.4 MPa1800 psiCure 1; ASTM D-638
 17.9 MPa2600 psiCure 2; ASTM D-638
Elongation at Break 425 %425 %Cure 2; ASTM D-638
 500 %500 %Cure 1; ASTM D-638
Tear Strength 47.3 kN/m270 pliCure 1; ASTM D-624
 48.2 kN/m275 pliCure 2; ASTM D-624
Taber Abrasion, mg/1000 Cycles  4.0
@Load 1.00 kg
4.0
@Load 2.20 lb
Cure 1, H-18 wheel; ASTM D-4060
 4.0
@Load 1.00 kg
4.0
@Load 2.20 lb
Cure 2, H-18 wheel; ASTM D-4060
 
Processing PropertiesMetricEnglishComments
Cure Time 240 - 360 min4.00 - 6.00 hourMix, Demold time
Gel Time 15.0 - 25.0 min15.0 - 25.0 minMix
 
Descriptive Properties
AspectAmberCure 1
 AmberCure 2
Mix Ratio100:40Resin: Hardener, Weight
 100:42Resin: Hardener, Volume
Split tear102ASTM D-470, Cure 1
 102ASTM D-470, Cure 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF099 / 317699

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.