MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.

Applications:

    Automotive: Bumper cover, instrument panel, glove box, air cleaner, mud guard, door trim, garnish

    Electrical and Electronic: Tail lamp housing, air conditioner housing, fan, socket, washing machine parts

    Industrial Parts and Household Appliance:Propeller fan, pulley, container, pump container, pump casing, handle and switch cover of electric jar, fan shroud/support

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Linear Mold Shrinkage 0.0090 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPaASTM D638
Elongation at Break 60 %ASTM D638
Flexural Strength 40.0 MPaASTM D790
Flexural Modulus 1.81 GPaASTM D790
Izod Impact, Notched 52.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 200 - 220 °C
Middle Barrel Temperature 200 - 230 °C
Front Barrel Temperature 210 - 230 °C
Nozzle Temperature 210 - 240 °C
Melt Temperature 210 - 240 °C
Mold Temperature 40.0 - 90.0 °C
Drying Temperature 70.0 - 90.0 °C
Dry Time 2 - 3 hour
Injection Pressure 29.4 - 118 MPaFirst
 78.45 - 98.07 MPaSecond
Back Pressure 0.490 - 3.92 MPa
Screw Speed 40 - 60 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed
A. Schulman Lucent CPP-0307 Polypropylene, Mineral Filled, Impact Modified
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant

PLGCHEM076 / 50897

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.