MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aperam IN540 Cold Rolled Strip Thermostatic bimetal (Corrosion resistance and protection)
Categories: Metal; Ferrous Metal

Material Notes: Aperam bimetals “IN540” find very wide application regarding its corrosion resistance, and is suitable for use in contact with water or steam atmosphere.

International standards: DIN-1715 , ASTM-B388

Typical Chemical composition:
Passive Component: Fe Ni38 Cr7
Active Component: Fe Ni19 Cr7

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.10 g/cc0.293 lb/in³
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00008075 - 0.00008925 ohm-cm0.00008075 - 0.00008925 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C
@Temperature -20.0 - 200 °C
5.56 µin/in-°F
@Temperature -4.00 - 392 °F
Maximum Service Temperature, Air 500 °C932 °F
 
Descriptive Properties
Spec thermal curvature17.6-19.42[10e-06/K°]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 5083-O
Sandvik 12C27 Strip Steel
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel
Aluminum 5652-O
Aluminum 5083-H32; 5083-H323

NPERA065 / 194854

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.