MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains its fibrous nature to 2480°C. The stabilized zirconia composition permits the advantages of fibrous insulations to be extended into temperature regions well above the melting temperatures of siliceous and alumina insulation materials.

Zirconia Felt Type ZYF-S.75G is ZYF-100 which has been physically filled with 0.75 grams silica per gram ZYF. This filled product retains some flexibility.

Features:

  • Low Thermal Conductivity
  • High Porosity
  • High Purity
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Custom Fillers and Coatings Available
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Rigidized with Zircar Zirconia Rigidizer Type ZIR-RIG
  • Easily Cut to Size
  • Available “Off the Shelf”

Application Information:

  • This heavy, silica loaded felt is used as a gasket material in molten carbonate fuel cells. When compressed between the sealing surfaces of the fuel cell container ZYF-S.75G forms a barrier that resists attack from the molten carbonate electrolyte.

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.4806 g/cc
Porosity 88 %Bulk
Thickness 70.0 - 130 mil
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength 0.0896 MPaAt 10% compression
 
Thermal PropertiesOriginal ValueComments
Shrinkage 5.0 %
@Temperature 1650 °C,
Time 3600 sec
1 hour isothermal soak at 3000°F
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 0.010 %
HfO2 1.0 - 2.0 %
SiO2 43 %
ZrO2+Y2O3 >= 56 %
 
Descriptive Properties
Tensile Strength per Unit Width1.7 lb/in width
Weight Per Area.22 lb/ft2
Wrapping Diameter Before Breaking>2 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation
Zircar Refractory Composites RS-3000 ALUMINA FELT
Thermal Ceramics K-Shield LS Felt
Sinotek Materials Graphite Felt Heat Insulation Material

C6ZIR017 / 2773

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.