MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow INSPIRE™ D7000 Thermoplastic Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes:

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Filler Content 24 %ISO 3451
Melt Flow 28 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70ISO 868
Tensile Strength, Yield 3220 psiISO R527
Flexural Modulus 305450 psiISO 178
Izod Impact, Notched (ISO) 30.0 kJ/m²NB; ISO 180/1A
 2.00 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 15.0 kJ/m²
@Temperature 10.0 °C
ISO 180/1A
Falling Dart Impact 34.0 J@ 23°C, 6.7 m/s; ASTM D3763
 36.1 J@ 0°C, 6.7 m/s; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 59.0 µm/m-°C
@Temperature 20.0 °C
ASTM D228
Deflection Temperature at 0.46 MPa (66 psi) 242.6 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 141.8 °FISO 75
Flame Spread 39.0 mm/min
 
Descriptive Properties
Five Finger Scratch (N)15

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow INSPIRE™ TF2300 Thermoplastic Polyolefin
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP)
Dow INSPIRE™ D7030EZ Thermoplastic Polyolefin
Dow INSPIRE™ DT701-14 Thermoplastic Polyolefin
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer

PDOW11504 / 30358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.