MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 EP Conolith® Grease NLGI NO. 0
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for these bearings when they are subjected to high speeds, moderate temperatures, water and shock loads. It does not contain any tackifiers, which makes it ideal for centralized lubrication systems. EP Conolith Grease is available in several NLGI grades and has been widely accepted in the steel, aluminum and other industries as a general-purpose plant grease. EP Conolith Grease is widely used by the can manufacturing industry because it has, in addition to the required performance characteristics, a light, low-staining, natural color. EP Conolith Grease is manufactured with high-viscosity index paraffinic basestocks and lithium 12-Hydroxy stearate soap stock. It is compounded with an effective extreme-pressure additive and corrosion inhibitors which impart good load-carrying characteristics and good chemical stability.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 95Viscosity Index
Saybolt Viscosity at 100°F 880 SUSBase Oil Property
Saybolt Viscosity at 210°F 86 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 190 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 17 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 250 kg
Four Ball Wear 0.410 mm
Penetration P(60), 1/10 mm 370
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air 0.000 °F
Pour Point 10.0 °F
Dropping Point 350 °F
 
Descriptive Properties
ASTM Rust A&BPass
ColorGreen/Brown
Low Temperature Mobility0.3 gm/secat 0°F
 1 gm/secat 10°F
 2.2 gm/secat 20°F
Shear Stability+2% in ConsistencyRoll Stability
Soap Type (Thickener)Lithium
Water Washout13%at 100°F
 32%at 175°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polygon Composites Polylube® HT High Temperature Bearings Versatile high load, low friction composite bearings
Phillips 66 EP Conolith® Grease NLGI NO. 1
Phillips 66 EP Conolith® Grease NLGI NO. 000
Phillips 66 EP Conolith® Grease NLGI NO. 00
Lubriplate Lithium Brick Grease Specialty Lubricant and Grease

WCON204 / 75241

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.