MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Tosoh TZ-8Y Zirconia powder
Categories: Other Engineering Material

Material Notes: Tosoh is utilizing powder technologies in the field of the high strength and high fracture toughness zirconia to supply fully stabilized zirconia powder for solid oxide fuel cell (SOFC). High-purity Tosoh powder provides sintered bodies which have superior electric properties. Tosoh powder has superior sintering properties and provides sintered bodies which have uniform grains.

Information provided by Tosh Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.90 g/cc
Specific Surface Area 13 - 19 m²/g
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 1250
@Load 10.00 kg
JIS R1610
Flexural Strength 300 MPa3-point bending test; JIS R1601
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 19.8 ohm-cm
@Temperature 800 °C
4-terminal method by direct current
 
Descriptive Properties
AppearanceGranule
Chemical Properties8 mol%Y2O3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOSOH095 / 306550

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.