MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® HL3712 Sheet and Thermoforming HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

Material Notes: Medium Density Hexene Copolymer

Applications: Gas and chemical tank containment liners, pond liners, landfill liners, tunnel liners.

Formolene HL3712 has good processability, excellent melt strength, broad fusion range, and outstanding stress-crack resistance.

Formolene HL3712 meets all requirements of ASTM D1248 - Type II, Class A, Category 5 and ASTM D4967-89-PE235.

Produced using licensor formulation for HHM TR 400G. Licensor does not warrant or imply that this product meets their specifications for HHM TR 400G.

Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.937 g/ccASTM D1505
ESCR 100% Igepal® >= 1500 hourCondition C, F50; ASTM D1693
ESCR 10% Igepal® >= 1500 hourCondition B, F50; ASTM D1693
High Load Melt Index 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2600 psi2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 700 %2" (50mm) per min.; ASTM D638
Flexural Modulus 120000 psiASTM D790

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® HL3721 Sheet and Thermoforming HDPE
Formosa Plastics Formolene® HB5502S1 Sheet and Thermoforming HDPE
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE
Chevron Phillips Marlex® K606 High Density Polyethylene
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE

PFPCPE22 / 38829

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.