MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese ZENITE SEA20N LCP, 40% Mineral Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: ZENITE« SEA20N is a 40% mineral filled grade. It offers excellent surface appearance, low warpage, and excellent dimensional stability. Application for this grade is compact camera module, and other thin, small electronic parts

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.768 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0025 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0076 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 105 MPa5mm/min; ISO 527-2/1A
Elongation at Break 4.2 %5mm/min
Tensile Modulus 10000 MPa50mm/min; ISO 527-2/1A
Flexural Strength 126 MPaISO 178
Flexural Modulus 10000 MPaISO 178
Charpy Impact, Notched 4.50 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 330 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 220 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 140 °Ccavity
Zone 1 310 - 320 °C
Zone 2 320 - 330 °C
Zone 3 330 - 350 °C
Zone 4 330 - 350 °C
Die Temperature 330 - 340 °C
Melt Temperature 335 - 345 °C
Drying Temperature >= 150 °C
Dry Time 6.00 hour
Injection Pressure 50.0 - 150 MPa
Hold Pressure 50.0 - 150 MPa
 
Descriptive Properties
Injection speedmedium-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese ZENITE 6635 LCP, 40% Mineral / Glass Reinforced (Extended Stress-Strain Tabular Data)
Celanese Zenite® 6635 BK010 LCP
Polyplastics TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
Celanese ZENITE 6330 LCP, 30% Mineral Reinforced

PHCQ545A / 183221

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.