MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil 320 Mobil SHC PM Series
Categories: Fluid; Lubricant

Material Notes: Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide exceptional lubrication characteristics not attainable with conventional premium mineral oil-based fluids. The Mobil SHC PM Series oils are formulated to provide maximum protection of gears and bearings operating under the most severe conditions. They have very low pour points and a naturally high viscosity index (VI) which helps ensure good low temperature start-up while maintaining excellent viscosity characteristics at very high temperatures. The fluids are very shear stable and maintain viscosity control even when subjected to severe mechanical shear in heavily loaded bearings and gears. Their low traction coefficient and high viscosity index can help result in lower energy consumption and reduced component operating temperatures. Mobil SHC PM Series oils are formulated with synthesised hydrocarbon fluid (SHF) base oil technology and a proprietary additive system carefully balanced to attain high performance standards These fluids permit the use of higher steam pressures, temperatures and machine speeds common in high output paper machines and calendar rolls. Their outstanding hydrolytic stability and filterability assure excellent performance in the presence of water and the ability to retain effective filtration even at very fine filtration levels. They readily separate water and retain their colour characteristics for extended periods of operation under severe conditions.

Lubrication of severe industrial paper machine circulating systems; Application involving circulation systems operating over a wide temperature range such as calendar rolls; Systems that must be started and brought on line quickly; Circulation systems lubricating gears and bearings

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.865 g/cc
@Temperature 15.0 °C
ASTM D1298
Viscosity Measurement >= 135Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 325 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 34.7 cStASTM D445
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.00Hydrolytic Stability (Acid Number Change), mgKOH/g; ASTM D2619
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -33.0 °CASTM D97
Flash Point >= 220 °CASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C
Demulsibility Time (min)30to 3 mL emulsion @ 82°C
FZG 4-Square Load Support, DIN 51354, Fail Stage11
Rust Prevention, Distilled WaterpassASTM D665A
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON272 / 75697

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.