MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Braskem HD3000N HDPE Cast Film Extrusion Polyethylene Homopolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: HD3000N is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for cast film extrusion. It offers high processability, stiffness, and good impact resistance. It contains a phenol free antioxidant additive. Its applications include cast film extrusion for diapers, hygienic absorbers, and other specialties. HD3000N is indicated for processing in a plain die extruding machine in conditions that are similar to the other types of high-density polyethylene of equivalent melt index and density. Recommended temperature range: 250 to 290 °C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM-D792
Melt Flow 7.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 770 %ASTM-D882
Film Elongation at Break, TD 380 %ASTM-D882
Elmendorf Tear Strength MD 5.0 gASTM-D1922
Elmendorf Tear Strength TD 10 gASTM-D1922
Film Tensile Strength at Break, MD 25.0 MPaASTM-D882
Film Tensile Strength at Break, TD 20.0 MPaASTM-D882
1% Secant Modulus, MD 710 MPaASTM-D882
1% Secant Modulus, TD 790 MPaASTM-D882
 
Optical PropertiesOriginal ValueComments
Haze 47 %ASTM-D1003
Gloss 52 %Angle 60°; ASTM-D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene
Bayport Polymers Baystar™ 6410 HDPE Film Resin
ExxonMobil Escorene® Escomer® H-101 Low MW HDPE Wax
LyondellBasell Lupolen UHM 201 MDPE, Ultra-High Molecular Weight
LyondellBasell Lupolen UHM 301 MDPE, Ultra-High Molecular Weight

PBRAS861 / 106707

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.