MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow Fusabond® E158 Polymer Modifier
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: DuPont™ Fusabond® E158 is a anhydride modified polyethylene.

Uses:

  • Adhesives
  • Pipe Coating
  • Tie-Layer

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 11.33 MPa1644 psiLap Shear; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Melting Point 113 °C235 °FFreezing Point; ASTM D3418
 128 °C262 °FASTM D3418
Vicat Softening Point 102 °C216 °FASTM D1525, ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 290 °C<= 554 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Fusabond® C190 Polymer Modifier
Dow Fusabond® E158H Polymer Modifier
Dow Fusabond® N416 Polymer Modifier
Dow Fusabond® A560 Polymer Modifier
Dow Fusabond® C250 Polymer Modifier

PDTA4958 / 170398

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.