MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinpolene MBW1444 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Sinpolene MBW1444 is a polypropylene-based pure white masterbatch designed specifically for use in injection molding and sheet extrusion of polypropylene. With its high pigment loading, it offers high coloring value with excellent quality and performance. The blue undertone of this masterbatch is attributed by specially selected high performance, fine crystal size rutile titanium dioxide. It is delivered as free flowing pellets for processing convenience.

Characteristic:

  • Easy processing
  • Good dispersion
  • Excellent whiteness
  • High opacifiying power
Availability: Asia Pacific

Filler/Reinforcement: Titanium Dioxide Equivalent, 50% Filler by Weight

Uses: Film; Masterbatch; Sheet

Agency Ratings:FDA Unspecified Rating

Form: Pellets

Processing Method: Injection Molding; Sheet Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ASTM D792
Maximum Moisture Content 0.200.20ASTM D3030
Melt Flow 10 - 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 - 30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Descriptive Properties
AppearanceWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HC101BF Polypropylene Homopolymer
Borealis HB205TF Polypropylene
ExxonMobil Label-Lyte™ 65LTR741 OPP Film
ExxonMobil Bicor™ 21MBT621 OPP Film
BP Amoco Amoco® 6361 Polypropylene Homopolymer

PTEKNQ1369 / 237860

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.