MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its excellent processing characteristics it is often used in complicated components. Typical applications include electrical cooling fans and housings, fuse boxes and carriers, flame retardant cable ties and corrugated tube. This product can be supplied in a full range of colors and has an excellent surface finish. For this reason it is often used in aesthetical components, like public bathroom accessories or trash cans.

Key characteristics:

  • Easy processing
  • Good heat aging characteristics: UL RTI listing (mechanical) up to 140°C
  • V0 listing at 0.75 mm
  • Halogen and red phosphorous free
  • Excellent CTI value (600 V)
  • Good impact strength
  • Good elongation

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792, ISO 1183
Water Absorption 2.0 %23°C, 24h in H2O; sim. ISO 62
Water Absorption at Saturation 9.0 %sim. ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cmEuronil
Linear Mold Shrinkage, Transverse 0.013 cm/cmEuronil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 80.0 MPaISO 527, ASTM D638
Elongation at Break 5.0 %ISO 527, ASTM D638
Tensile Modulus 2.70 GPaISO 527, ASTM D638
Flexural Yield Strength 115 MPaISO 178, ASTM D790
 50.0 MPa
@Temperature 90.0 °C
ISO 178, ASTM D790
Flexural Modulus 2.90 GPaISO 178, ASTM D790
 0.700 GPa
@Temperature 90.0 °C
ISO 178, ASTM D790
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 12.0 J/cm²ISO 179
 6.00 J/cm²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.500 J/cm²ISO 179
 0.300 J/cm²
@Temperature -30.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 18.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Comparative Tracking Index 550 V
@Thickness 3.20 mm
Sol. B; IEC 112, UL 746A
 600 V
@Thickness 3.20 mm
Sol. A; IEC 112, UL 746A
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 190 °CISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CISO 75, ASTM D648
Vicat Softening Point 196 °C49 N; ISO 306, ASTM D1525
 210 °C9.8 N; ISO 306, ASTM D1525
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
Oxygen Index 29 %ASTM D2863
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
IEC 694-2-12
 960 °C
@Thickness 0.800 mm
IEC 694-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 455 - 509 °F
Zone 1 437 - 482 °Fhopper
Zone 2 446 - 509 °F
Zone 3 455 - 509 °F
Zone 4 455 - 509 °F
Melt Temperature 230 - 260 °CDo not melt above 275°C
Mold Temperature 60.0 - 80.0 °C80°C is Preferred
Drying Temperature 80.0 - 85.0 °C
Dry Time 4 hour
Injection Pressure 70.0 - 100 MPa
 
Descriptive Properties
Clamping Forcein tons, 0.7 times the projected surface area in cm2
Flammability RatingSEFMVSS No. 302, 355x100x1 mm
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309
Holding Pressure90 MPa
Needle TestOKIEC 695-2-2, 1 or 2 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® C 50 H2 PA6, DRY
EMS-Grivory Grilon® BS V0 PA6
Envalior Akulon® K225-KWS (Dry) Nylon 6 (North America)
Envalior Arnitel® CM600-V TPC-ES FR, Extrusion, Flame Retardant
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant

PLBN55 / 50444

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.