MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lion Royalene® 515 EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: An Ultra Fast Curing Polymer for Automotive Extrusions

Unique Features:

  • High unsaturation - Ultra fast cure rate
  • Excellent compression set resistance in closed cell sponge extrusions
  • Excellent low temperature properties
  • Co-cures well with SBR
  • Non-staining
  • Friable bale form for rapid mixing in internal mixers and excellent dispersion properties
  • Excellent weathering resistance
Applications:
  • Closed cell sponge profile extrusions
  • Closed cell sheet sponge
  • Automotive window channel extrusions

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.860 g/ccASTM D-792
Volatiles <= 0.70 %ZS 1008K
Mooney Viscosity 82
@Temperature 150 °C
ML (1+4), Unmilled; ZS 1220C
 
Descriptive Properties
ColorOff-whiteZS 1072A
Content0.095ENB, ZS 1222
StabilizerNon-Staining
Weight Ratio62/38E/P, ZS 1231

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLION006 / 317915

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.