MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® 20-0778/BK Polyphthalamide with glass fiber and PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Glass/PTFE Filled

Material Notes: Properties/attributes include: Very strong and stiff parts; low coefficient of thermal expansion. Low influence from moisture and temperature to measures and electrical properties, compared with PA66 Suitable for metal inserts. Improved friction and wear behavior. Emergency (dry) running property.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.

Processing: During processing the moisture level should not exceed 0.05%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Processing temperatures above 340°C may very rapidly cause thermal damage and should therefore be avoided. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.56 g/ccISO 1183
Moisture Absorption <= 0.300 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmDIN 16901
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 195 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Modulus of Elasticity 12.0 GPaISO 527-2
Flexural Strength 275 MPaISO 178
Flexural Modulus 10.0 GPaISO 178
Flexural Strain at Break 2.5 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1fu
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cmIEC 60167
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °CContinuous; UL 746B
 195 °CShort Term
Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-2/A
Vicat Softening Point 295 °CVST A; DIN ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 320 - 330 °C
Zone 1 320 - 340 °C
Zone 2 320 - 345 °C
Zone 3 325 - 350 °C
Melt Temperature 330 °C
Mold Temperature 135 - 160 °C
Drying Temperature 80.0 °C
@Time >=57600 sec
Dehumidifying dryer
 105 °C
@Time 14400 - 18000 sec
Vacuum Dryer
Moisture Content <= 0.050 %
 
Descriptive Properties
Colorblack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 4002 Polyphthalamide (PPA), Glass Fiber
Techmer ES Luriblend® PPA CF30 TL10 30% Carbon Filled
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled
RTP Company RTP 4081 TFE 5 Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled

PLUU8910 / 193869

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.