Hostacom EKG 2130-2L BLACK is a 20% glass fiber reinforced PP (coupled). It combines excellent stiffness properties with good dimensional stability and low creep under load at elevated temperatures. Product is UL certified. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: White Goods Market: Electrical / Electronics Processing Method: Injection Molding Information provided by LyondellBasell. |