MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Hifax™ CB276 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of properties and processability. It was designed for exterior applications that require good cosmetics and undergo prolonged outdoor exposure. Uses: Automotive exterior parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 17.0 MPa2470 psiISO 527-1, -2
Elongation at Yield 13 %13 %ISO 527-1, -2
Flexural Modulus 1.20 GPa174 ksiISO 178
Izod Impact, Notched (ISO)  3.20 kJ/m²
@Temperature -40.0 °C
1.52 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 28.0 kJ/m²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Dart Drop, Total Energy 21.0 J
@Temperature 0.000 °C
15.5 ft-lb
@Temperature 32.0 °F
Peak Energy, 135.0 m/min; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature -30.0 - 100 °C
38.9 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 77.2 °C171 °FUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C118 °FUnannealed; ISO 75A-1, -2
Shrinkage 0.70 %0.70 %Tool, 100x150x3.2 mm; Basell Test Method
 1.1 %
@Temperature 121 °C,
Time 3600 sec
1.1 %
@Temperature 250 °F,
Time 1.00 hour
Afterbake, 100x150x3.2 mm; Basell Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elastocon TPE Technologies Elastocon® SMR1000 Thermoplastic Polyolefin Elastomer
Dow Engage® 8401 Polyolefin Elastomer
Celanese SO.F.TER Pibiflex® L 6360 NAT Copolyester TPE
Celanese SO.F.TER Laprene® 830.951 TPE
Celanese SO.F.TER Laprene® 830.541 TPE

PMO790 / 53779

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.