System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Celanex® 4300 PBT, 30% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Material Notes:
Celanex 4300 is a toughened, 30% glass reinforced PBT.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.53
g/cc
1.53
g/cc
ASTM D792
Density
1.53
g/cc
0.0553
lb/in³
ISO 1183
Moisture Absorption
0.140 %
0.140 %
23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow
0.0030
-
0.0050
cm/cm
0.0030
-
0.0050
in/in
ISO 294-4
0.0030
-
0.0050
cm/cm
0.0030
-
0.0050
in/in
ASTM D955
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
0.0080
in/in
ISO 294-4
Melt Flow
7.0
g/10 min
7.0
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
91
91
ISO 2039-2
Tensile Strength at Break
124
MPa
18000
psi
ASTM D638
130
MPa
18900
psi
5mm/min; ISO 527-2/1A
Elongation at Break
3.0 %
3.0 %
ASTM D638
3.1 %
3.1 %
5mm/min; ISO 527-2/1A
Tensile Modulus
9.30
GPa
1350
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
186
MPa
27000
psi
ASTM D790
205
MPa
29700
psi
ISO 178
Flexural Modulus
8.27
GPa
1200
ksi
ASTM D790
9.00
GPa
1310
ksi
ISO 178
Izod Impact, Notched
1.01
J/cm
1.90
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
12.1
kJ/m²
5.76
ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched
4.00
J/cm²
19.0
ft-lb/in²
ISO 179/1eU
5.10
J/cm²
@Temperature -30.0 °C
24.3
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
1.09
J/cm²
5.19
ft-lb/in²
ISO 179/1eA
0.850
J/cm²
@Temperature -30.0 °C
4.04
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
IEC 60093
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Surface Resistance
1.00e+15
ohm
1.00e+15
ohm
IEC 60093
Dielectric Constant
2.8
@Frequency 100 Hz
2.8
@Frequency 100 Hz
IEC 60250
3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
ASTM D150
3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
20.0
kV/mm
508
kV/in
IEC 60243-1
21.7
kV/mm
550
kV/in
short term; ASTM D149
Dissipation Factor
0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
0.022
@Frequency 1e+6 Hz
0.022
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
400
V
400
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
24.0
µm/m-°C
13.3
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
80.0
µm/m-°C
44.4
µin/in-°F
ISO 11359-2
Melting Point
225
°C
437
°F
10°C/min; ISO 11357-1,-2,-3
225
°C
437
°F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
428
°F
ISO 75-1, -2
223
°C
433
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
200
°C
392
°F
ISO 75-1, -2
204
°C
399
°F
ASTM D648
Glass Transition Temp, Tg
41.0
°C
106
°F
ISO 11357-1,-2,-3
Flammability, UL94
HB
@Thickness 0.710 mm
HB
@Thickness 0.0280 in
Processing Properties
Metric
English
Comments
Processing Temperature
65.0
-
93.0
°C
149
-
199
°F
cavity
250
-
260
°C
482
-
500
°F
hot runner
Feed Temperature
230
-
240
°C
446
-
464
°F
Zone 1
230
-
240
°C
446
-
464
°F
Zone 2
235
-
250
°C
455
-
482
°F
Zone 3
235
-
250
°C
455
-
482
°F
Zone 4
240
-
260
°C
464
-
500
°F
Die Temperature
250
-
260
°C
482
-
500
°F
Melt Temperature
235
-
260
°C
455
-
500
°F
260
°C
500
°F
ISO 294
Mold Temperature
82.0
°C
180
°F
ISO 294
Injection Velocity
300
mm/sec
11.8
in/sec
ISO 294
Drying Temperature
120
-
130
°C
248
-
266
°F
Dry Time
4.00
hour
4.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Hold Pressure
48.0
MPa
6960
psi
ISO 294
Descriptive Properties
Injection molding
Yes
Injection speed
medium-fast
Processing conditions acc. ISO
7792-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Dow LIGHTER™ C93 Polyethylene Terephthalate (PET) Resin
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA
Celanese Celanex® 3300-2 PBT, 30% Glass Reinforced
Celanese Celanex® 2302 GV1/30 PBT, 30% Glass Reinforced
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT
PHCQ066 / 178521
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.