MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
CHT Primer No. 6 Primer
Categories: Other Engineering Material

Material Notes: Description: This is a specially formulated silicone based primer for use with a wide range of CHT 1K Condensation / Moisture curing RTV silicone sealants. This primer imparts good adhesion to most metals. It is recommended as a primer for use on non-porous surfaces. For all new applications, it is recommended that customers carry out small-scale tests to determine the suitability of the primer and the strength of bond produced.

Key Features

  • Aerospace approved
  • Suitable for use with CHT adhesives
  • Suitable for non porous surfaces
  • For use with most metals
Key Applications
  • Rolls Royce MSRR1064
Application: Primer for condensation cure 1 part adhesives on metal substrates. Not suitable for polycarbonate and acrylic

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.830 g/ccBS ISO 2781
Brookfield Viscosity 1.0 cP
Storage Temperature 5.00 - 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point 28.0 °CBS 2000-34
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 minTack Free Time / Skin Formation
Shelf Life 12.0 Month
 
Descriptive Properties
ColorPale Yellow
RheologyLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL393 / 314876

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.