MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexBond™ 679 400g/m2 Supported Epoxy Film Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: HexBond™ 679 is a modified epoxy film adhesive, designed for low temperature cure in out-of-autoclave applications. It contains a 30 g/m2 non-woven polyester/glass support for easy handling and bond-line thickness control. The product offers higher tack and lower cure viscosity to aid with substrate wetting. It is available with a resin areal weight of 150, 250 and 400 g/m2.

Features:

  • Fully compatible with HexPly® M79 o Cure cycle as low as 70°C for 8 hours (typically 4 hours @ 80°C)
    • Well adapted to a wide range of processing pressures (0.3 – 5 bar)
    • Diuron-free chemistry
    • Less than 1% volatile content
  • Suitable for bonding a wide range of substrates (-55°C to 80°C)
    • Good lap shear and peel performance
    • Outstanding properties in sandwich structures (honeycomb & foam cores)
  • Excellent tack life to assist in adhesive joint assembly
  • Superior shelf-life (6 weeks @ +23°C)
  • Translucent resin after cure for easy quality inspection
Applications:
  • Aluminum to aluminum bonding
  • Steel to steel bonding
  • CFRP/GFRP to CFRP/GFRP bonding
  • CFRP and GFRP to aluminum bonding
  • CFRP and GFRP to steel bonding
  • Sandwich bonding with a variety of skins and cores (e.g. PVC, VE, glass, polyester, aluminum, steel)

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 - 1.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 29.0 MPaLap Shear, Aluminum; BS EN 2243-1
 29.0 MPaLap Shear, Steel; BS EN 2243-1
Peel Strength 9.84 kN/mClimbing Drum
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 85.0 - 95.0 °CTypical cured, following 130min @ 90°C
 95.0 - 105 °COptimum cured Tg, following 120min @ 100°C
 
Processing PropertiesOriginal ValueComments
Cure Time >= 60.0 min
@Temperature 110 °C
ISO 11357-5
 >= 60.0 min
@Temperature 120 °C
ISO 11357-5
 >= 80.0 min
@Temperature 100 °C
ISO 11357-5
 >= 140 min
@Temperature 90.0 °C
ISO 11357-5
 >= 240 min
@Temperature 80.0 °C
ISO 11357-5
 >= 480 min
@Temperature 70.0 °C
ISO 11357-5
Shelf Life 0.750 Month
@Temperature 30.0 °C
 1.50 Month
@Temperature 23.0 °C
 6.00 Month
@Temperature 5.00 °C
 18.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Coloroff-white – yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9281 / 322437

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.