MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kazanorgsintez Phenol, Synthetic, Commercial
Categories: Fluid

Material Notes: Obtained by the cumene method.

Application: The product is used in the production of caprolactam, diphenylpropane, medicines, phenol, formaldehyde resins, orthocresol, and oil additives, for selective purification of oils and for other applications.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles >= 0.99 %>= 0.99 %Grade H
 >= 0.992 %>= 0.992 %Grade B
 >= 0.999 %>= 0.999 %Grade A
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature >= 40.4 °C>= 105 °FGrade H
 >= 40.6 °C>= 105 °FGrade B
 >= 40.7 °C>= 105 °FGrade A
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 0.030 %<= 0.030 %Grade A
 
Descriptive Properties
Amount of impurities [pcs]0.01Grade A, Organic impurities
AppearanceWhite crystal substance (pinkish or yellowish shade is allowed in Grade H)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haveg 41NA Phenolic; Silicate Filled
Vitreous Carbon (Glassy Carbon)
Lanxess Nigrosin W liq Acid Black 2
Kazanorgsintez Phenol Resin
Total XT10 N High Density Polyethylene - Pipe Resin

PKAZAN178 / 127497

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.