The AD1/CS Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS as well as excellent compression set. The compounds are available in natural and black colors. Typical applications: - Ear phones
- Fastenings
- Grommets
- Membranes
- Seals
Material advantages:- Easy coloring (compounds in natural colors)
- Excellent compression set
- Insert molding possible
- UL 94 HB listed
Processing Method: Extrusion, Injection MoldingInformation provided by Kraiburg TPE. A newer data sheet is available in MatWeb. |