Varcum 29407 is a one-step crushed phenolic resin. APPLICATION: Formulation of acrylonitrile rubber adhesive systems. FEATURES: - Provides light color.
- Exhibits good balance between strength and heat resistance.
- Compatible with many rubbers and solvents.
- Imparts high resistance to ultra-violet staining.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |