MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Vespel® SP-211 Polyimide, 15% Graphite, 10% Teflon® Filled, Machined
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Has lowest coefficient of friction over wide range of operating conditions. Also, has lowest wear rate up to 300°F.

Applications: For low friction and wear applications in moderate temperature and PV environments. Bearings (bushings, washers, etc.).

Direct-formed properties were measured perpendicular to the forming direction unless specified. Machined properties are non-directional

Information provided by DuPont

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/ccASTM D792
Water Absorption 0.21 %24 hrs @ 73°F.; ASTM D570
 0.49 %48 hrs @ 122°F; ASTM D570
Deformation 0.13 %2000 psi; 122°F; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E <= 20ASTM D785
Tensile Strength, Ultimate 6500 psi73°F; ASTM D1708
 3500 psi
@Temperature 260 °C
ASTM D1708
Elongation at Break 3.5 %73°F; ASTM D1708
 3.0 %
@Temperature 260 °C
ASTM D1708
Flexural Strength 5000 psi500°F; ASTM D790
 10000 psi73°F; ASTM D790
Flexural Modulus 200 ksi500°F; ASTM D790
 450 ksi73°F; ASTM D790
Compressive Strength 3000 psi@1% strain; 73°F; ASTM D695
 5400 psi@0.1% Offset; 73°F; ASTM D695
 14800 psi@10% strain; 73°F; ASTM D695
Compressive Modulus 300000 psi73°F; ASTM D695
Coefficient of Friction, Dynamic 0.080PV-100,000. Steady State; Unlubricated in air.
 0.12PV-25,000. Steady State; Unlubricated in air.
Coefficient of Friction, Static 0.20In air.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µin/in-°F
@Temperature 22.8 - 300 °C
ASTM E-228
Thermal Conductivity 5.30 BTU-in/hr-ft²-°F104°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® PTFE
Fluorseals PTFE Unfilled
DuPont Mobility and Materials Vespel® SF-0940 Polyimide Foam, High Density
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI)
Overview of materials for Polytetrafluoroethylene (PTFE), Molded

PDU2006 / 32867

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.