MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TTC Taita TAITALAC® 1250 ABS, Impact Modified
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Characteristics:
  • Injection / extrusion
  • Medium high impact
  • Good flow for process
  • Metal platings
Applications:
  • Automobile grill
  • Various ornaments
  • Plating Wheel cap / radiator grille
  • Electric appliances

Information provided by Taita Chemical Company, Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccISO 1183
Moisture Absorption at Equilibrium <= 0.30 %<= 0.30 %C/50% RH; ISO 62
Linear Mold Shrinkage <= 0.0040 cm/cm<= 0.0040 in/in60×60×2mm Sflow; ISO 294-4
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
20 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ISO 2039-2
Tensile Strength at Break 32.0 MPa4640 psi50 mm/min; ISO 527
Tensile Strength, Yield 42.0 MPa6090 psi50 mm/min; ISO 527
Elongation at Break 30 %30 %50 mm/min; ISO 527
Flexural Yield Strength 66.0 MPa9570 psi2.0 mm/min; ISO 178
Flexural Modulus 2.00 GPa290 ksi2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²10.5 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²ISO 179/1A
 
Electrical PropertiesMetricEnglishComments
Hot Wire Ignition, HWI 17 sec
@Thickness <=1.57 mm
17 sec
@Thickness <=0.0620 in
UL-746A
High Amp Arc Ignition, HAI 200 arcs
@Thickness <=1.57 mm
200 arcs
@Thickness <=0.0620 in
UL-746A
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/min
@Thickness <=1.57 mm
0.000 in/min
@Thickness <=0.0620 in
UL-746A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °Funannealing; ISO 75
Vicat Softening Point 100 °C
@Load 1.00 kg
212 °F
@Load 2.20 lb
50°C/hr; ISO 306
UL RTI, Electrical 60.0 °C
@Thickness <=1.57 mm
140 °F
@Thickness <=0.0620 in
UL-746B
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTTC015 / 281535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.