MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Lescalloy® UT-18 VAC-ARC ; 6 in. round High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting is employed to provide a preferred ingot solidification and superior microcleanliness

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 205 ksi
Tensile Strength, Yield 1172 - 1186 MPa
@Strain 0.2 %
Elongation at Break 16 %
Reduction of Area 59 - 60 %
Izod Impact Notched 25.0 - 28.0 ft-lbV-Notch
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 3.25 %
Iron, Fe 94.3 %
Manganese, Mn 0.60 %
Molybdenum, Mo 1.0 %
Silicon, Si 0.25 %
Vanadium, V 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lescalloy® UT-18 VAC-ARC ; 1.25 in. round High Strength Alloy Steel
ASTM A470-8 1Cr-1Mo-0.25V STEEL FORGINGS FOR TURBINE ROTORS AND SHAFTS (ASTM A470-8)
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® 4340 VAC-ARC ; 3.5" round High Strength Alloy Steel
Latrobe Lescalloy® UT-18 VAC-ARC ; 4 in. round High Strength Alloy Steel

NTIMK040 / 19388

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.