MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aurora Plastics TufFill™ GPP3003FD Natural Flame Retardant concentrate in Polyethylene
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Flame Retardant Concentrate in Polyethylene. GPP3003FD is PE based, flame retardant concentrate, with 1.61 g/cm3 Gravity, designed to impart flame resistance to polyolefin. Dependent upon let-down ratio in extrusion or molding grade resins, GPP3003FD can provide a range of V-2 to V-0 flammability UL-94 ratings. GPP3003FD performance in a specific resin system may be submitted to Underwriters Laboratories for confirmatory UL Recognition

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.161 g/cc
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-2 - V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE 7A Granular Molding Powder
AISI 1030 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1030 Steel, as rolled
Firestone C200-001 Nylon 6
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm

PSEPN001 / 179005

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.