MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Network Polymers SBS 1000 Clear Styrene Butadiene Copolymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Polystyrene (PS); Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Description: Clear Styrene Butadiene Copolymer

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cmASTM D955
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60 - 70ASTM D2240
Tensile Strength at Break 3300 psichs 2 in/min; ASTM D638
Flexural Strength 5400 psiTest Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Flexural Modulus 250000 psiTest Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 0.500 ft-lb/in0.125 inch bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 76.9 °C0.125 in bar; ASTM D648
Vicat Softening Point 90.7 °C0.125 inch bar, 1 Kg; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Styrene/Butadiene/Styrene (SBS)
Chi Mei Kibiton® PB-5910 SBC
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer
RTP Company RTP 2740U-80A  Saturated Styrenic Elastomer (SBS) 80 Shore A
Asahi Kasei DELPET™ 720V Acrylic (PMMA), Standard Grade

PDIAM048 / 29886

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.