MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton ARC HT-S High Temperature Corrosion Resistant Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with conventional airless equipment. Spark testable, non-shrinking 100% solids. ARC HT-S is reinforced with high modulus reinforcements to improve long term resistance to cold wall induced blistering and delamination. Its unique chemistry allows for reliable long term immersion service at elevated temperatures without the need for post curing thereby simplifying installation. ARC HT-S is capable of in-situ curing.

Benefits:

  • High voltage spark testable to NACE SP 0188
  • Capable of ambient cure
  • Two color system provides visual indicators of mixing
  • Able to handle immersion in elevated temperature aqueous applications

Suggested Uses:

  • Process Cooling Water Heat Exchangers
  • Crystallizers/Evaporators
  • Centrifuges
  • Condensate Return Pumps
  • Distillation Units
  • Oil/Water, Oil/Gas Separator Vessels

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ASTM D2240
Tensile Strength at Break 31.0 MPa4500 psiASTM D638
Elongation at Break 2.2 %2.2 %ASTM D638
Flexural Strength 40.0 MPa5800 psiASTM D790
Flexural Modulus 3.10 GPa450 ksiASTM D790
Compressive Strength 106 MPa15400 psiASTM D790
Adhesive Bond Strength >= 13.8 MPa>= 2000 psiASTM D4541
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °FWet Service
 175 °C347 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  180 min
@Temperature 32.0 °C
3.00 hour
@Temperature 89.6 °F
Overcoat Begin
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
Overcoat Begin
 360 min
@Temperature 16.0 °C
6.00 hour
@Temperature 60.8 °F
Overcoat Begin
 480 min
@Temperature 10.0 °C
8.00 hour
@Temperature 50.0 °F
Overcoat Begin
 720 min
@Temperature 32.0 °C
12.0 hour
@Temperature 89.6 °F
Overcoat End
 1080 min
@Temperature 25.0 °C
18.0 hour
@Temperature 77.0 °F
Overcoat End
 1440 min
@Temperature 16.0 °C
24.0 hour
@Temperature 60.8 °F
Overcoat End
 1800 min
@Temperature 10.0 °C
30.0 hour
@Temperature 50.0 °F
Overcoat End
 4320 min
@Temperature 32.0 °C
72.0 hour
@Temperature 89.6 °F
Full Mechanical
 4320 min
@Temperature 32.0 °C
72.0 hour
@Temperature 89.6 °F
Full Chemical
 5760 min
@Temperature 25.0 °C
96.0 hour
@Temperature 77.0 °F
Full Mechanical
 5760 min
@Temperature 25.0 °C
96.0 hour
@Temperature 77.0 °F
Full Chemical
 7200 min
@Temperature 16.0 °C
120 hour
@Temperature 60.8 °F
Full Mechanical
 7200 min
@Temperature 16.0 °C
120 hour
@Temperature 60.8 °F
Full Chemical
 8640 min
@Temperature 10.0 °C
144 hour
@Temperature 50.0 °F
Full Mechanical
 8640 min
@Temperature 10.0 °C
144 hour
@Temperature 50.0 °F
Full Chemical
Tack-Free Time  240 min
@Temperature 32.0 °C
4.00 hour
@Temperature 89.6 °F
 360 min
@Temperature 25.0 °C
6.00 hour
@Temperature 77.0 °F
 480 min
@Temperature 16.0 °C
8.00 hour
@Temperature 60.8 °F
 600 min
@Temperature 10.0 °C
10.0 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorBlue
 Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Imerys 325D Ground Mica
Mica (KAl2(AlSi3O10)(OH)2)

PPTCHS043 / 138155

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.