Unreinforced nucleated heat-stabilized nylon 6/6 molding resin. Has the high heat and chemical resistance characteristic of nylon 6/6 materials, combined with nucleation for faster part set-up. Suitable for a variety of applications, such as clips, fasteners, levers, bushings, and other uses where heat, chemical, and wear resistance are required. Testing conducted on dry as molded specimen at 73°F Information provided by Nylene® Global Polymer Solutions. |