MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay JAGUAR® 413 Surfactant
Categories: Fluid

Material Notes: Description: Nonyl phenol based non ionic surfactant (70 EO)

Chemical Name: GALACTOMANNAN BLEND

CAS: 39421-75-5; 7631-86-9

Available in: Asia Pacific, Europe, Latin America and North America

Applications: JAGUAR® 413 is a highly substituted hydroxypropyl guar designed for thickening alcohol based fracturing fluids

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³
Particle Size 95 - 100 µm95 - 100 µm150 Mesh; PS-1-2
pH 9.0 - 119.0 - 110.6% aq sol
 5.0 - 7.0
@Time 3600 sec
5.0 - 7.0
@Time 1.00 hour
V-135-1
Viscosity  >= 14 cP
@Time 601 sec
>= 14 cP
@Time 0.167 hour
V-135-1
 >= 19 cP
@Time 3600 sec
>= 19 cP
@Time 1.00 hour
V-135-1
 >= 19 cP
@Time 86400 sec
>= 19 cP
@Time 24.0 hour
V-135-1
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 6.0 - 12 %6.0 - 12 %M-1-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MACKAZOLINE® O-V Surfactant
Solvay MACKANATE® OPV Surfactant
Solvay MACKAM® 2CYSF Surfactant
Solvay MACKADET® EQ-178 Surfactant
Solvay JAGUAR® C 14 S Surfactant

WRHOD170 / 137401

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.