A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin contains a lubrication package for improved release from the mold and lower application torques on the bottles. This material meets the FDA requirements of 21CFR 177.1520. |
Narrow molecular weight distribution; lubrication package |