MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pyrocast PT-190 Refractory Cast Parts
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resistant characteristics. Pyrocast PT-190 also provides excellent hot load strength. Pyrocast PT-190 is frequently used for applications such as launders, tap out and burner blocks, and door blades.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00800 GPa
@Temperature >=110 °C
 0.0220 GPa
@Temperature 1095 °C
 0.0300 GPa
@Temperature 1370 °C
Flexural Strength 22.0 MPa
Compressive Strength 31.0 MPa
@Temperature 110 °C
 110 MPa
@Temperature 1095 °C
 166 MPa
@Temperature 1370 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.84 W/m-K
@Temperature 1093 °C
 1.94 W/m-K
@Temperature 815 °C
 2.24 W/m-K
@Temperature 538 °C
 2.71 W/m-K
@Temperature 260 °C
Maximum Service Temperature, Air 1540 °C
Shrinkage 0.10 %
@Temperature 1090 °C
Linear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast AR-S Castable Refractory
Pyrotek Pyrocast AR70 Low-Density Refractory Castable
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast XL Small Component Refractory

CPYRO067 / 1806

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.